Nanomaterials mimicking the nano-features of bones and offering unique smart functions are promising for better bone fracture repair. This review provides an overview of the current state-of-the-art research in developing and using nanomaterials for better bone fracture repair.
This review begins with a brief introduction of bone fracture repair processes, then discusses the importance of vascularization, the role of growth factors in bone fracture repair, and the failure of bone fracture repair. Next, the review discusses the applications of nanomaterials for bone fracture repair, with a focus on the recent breakthroughs such as nanomaterials leading to precise immobilization of growth factors at the molecular level, promoting vascularization without the use of growth factors, and re-loading therapeutic agents after implantation.
The review concludes with perspectives on challenges and future directions for developing nanomaterials for improved bone fracture repair.