.....an insulating version of single-atom-thick graphene expected to find use in all kinds of material and electronic applications.
And a second paper shows how GO is broken down by common bacteria that leave behind only harmless, natural graphite. The papers appear online in the journal ACS Nano; [Marcano et al., ACS Nano., (2010), DOI:10.1021/nn1006368], and [Salas et al., ACS Nano., (2010), DOI:10.1021/nn101081t].
"These are the pillars that make graphene oxide production practical," said Tour, one of the lead authors. The GO manufacturing process was developed as part of a research project with M-I SWACO, a Houston-based producer of drilling fluids for the petrochemical industry that hopes to use graphene to improve the productivity of wells.
Scientists have been making GO since the 19th century, but the new process eliminates a significant stumbling block to bulk production, Tour said. "People were using potassium chlorate or sodium nitrates that release toxic gases – one of which, chlorine dioxide, is explosive," he said. "Manufacturers are always reluctant to go to a large scale with any process that generates explosive intermediates."
Tour and colleagues processed flakes of graphite – pencil lead – with potassium permanganate, sulfuric acid and phosphoric acid, all common, inexpensive chemicals.
"Many companies have started to make graphene and graphene oxide, and I think they're going to be very hard pressed to come up with a cheaper procedure that's this efficient and as safe and environmentally friendly," Tour said.
The researchers suggested the water-soluble product could find use in polymers, ceramics and metals, as thin films for electronics, as drug-delivery devices and for hydrogen storage, as well as for oil and gas recovery.
With so many potential paths into the environment, the fate of GO nanomaterials concerned Tour, who sought the advice of Rice colleague Lüttge.
Lüttge and Everett Salas, a postdoctoral researcher in his lab and primary author of the second paper, had already been studying the effects of bacteria on carbon, so it was simple to shift their attention to GO. They found bacteria from the genus Shewanella easily convert GO to harmless graphene. The graphene then stacks itself into graphite.
"That's a big plus for green nano, because these ubiquitous bacteria are quickly converting GO into an environmentally benign mineral," Tour said.