This graphic shows the charge transfer (e-) mechanism of fluorescent molecules (top) interacting with N-doped graphene (bottom sheet) when excited with different laser lines, producing an ultrasensitive molecular sensor. The white, blue and red balls represent carbon, nitrogen and oxygen respectively. Image: Terrones Lab, Penn State.
This graphic shows the charge transfer (e-) mechanism of fluorescent molecules (top) interacting with N-doped graphene (bottom sheet) when excited with different laser lines, producing an ultrasensitive molecular sensor. The white, blue and red balls represent carbon, nitrogen and oxygen respectively. Image: Terrones Lab, Penn State.

A highly sensitive chemical sensor based on Raman spectroscopy that uses nitrogen (N)-doped graphene as a substrate has been developed by an international team of researchers working at Penn State.

By introducing nitrogen atoms into the carbon structure of graphene, the researchers were able to produce a sensor that can detect trace amounts of molecules in solution at very low concentrations, some 10,000 times more diluted than can be seen by the naked eye.

Raman spectroscopy is a popular analytical technique used in chemistry, materials science and the pharmaceutical industry to detect the unique internal vibrations of various molecules. Irradiating crystals or molecules with light from a laser causes the light to scatter and shift colors. That scattered light can be detected in the form of a Raman spectrum, which serves almost as a fingerprint for every Raman-active irradiated system.

"Basically, different colors in the visible spectrum will be associated to different energies," explained Mauricio Terrones, professor of physics, chemistry and materials science at Penn State, who led the research. "Imagine each molecule has a particular light color emission, sometimes yellow, sometimes green. That color is associated with a discrete energy."

On its own, the Raman signal is so weak that many methods have been used to enhance the signal. A recently developed enhancement technique uses pristine graphene as a substrate, which can enhance the Raman signal by several orders of magnitude. In a paper recently published in Science Advances, Terrones and his colleagues revealed that adding nitrogen atoms to the pristine graphene further enhances its sensitivity and, importantly, they gave a theoretical explanation for how graphene and N-doped graphene causes the enhancement.

"By controlling nitrogen doping we can shift the energy gap of the graphene, and the shift creates a resonance effect that significantly enhances the molecule's vibrational Raman modes," said lead author Simin Feng, a graduate student in Terrones' group.

"This is foundational research," said Ana Laura Elias, a co-author and research associate in Terrones' lab. "It is hard to quantify the enhancement because it will be different for every material and color of light. But in some cases, we are going from zero to something we can detect for the first time. You can see a lot of features and study a lot of physics then. To me, the most important aspect of this work is our understanding of the phenomenon. That will lead to improvements in the technique."

"We carried out extensive theoretical and experimental work," added Terrones. "We came up with an explanation of why nitrogen-doped graphene works much better than regular graphene. I think it's a breakthrough, because in our paper we explain the mechanism of detecting certain molecules."

Because of graphene's chemical inertness and biocompatibility, the team expects the new technique to be effective at detecting trace amounts of organic molecules. Elias is excited about the prospect of combining the technique with available portable Raman spectrometers that can be taken to remote places to detect dangerous viruses, for example. Because the technique is simple – just dip the graphene substrate into a solution for a short amount of time – it should be feasible to create an entire library made up of the Raman spectra for specific molecules, Terrones said.

Researchers from Brazil, China and Japan contributed to this work while visiting the Terrones lab at Penn State.

This story is adapted from material from Penn State, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.