Sicomin, a supplier of epoxy systems, has developed InfuGreen 810 infusion system, which has recently been awarded DNV GL certification.

InfuGreen 810 is an advanced resin system with very low viscosity at room temperature and approximately 38% carbon content derived from plant based origins. It is available with a variety of hardeners and is suitable for small to very large components including thick laminates. The product has been formulated to support manufacturers producing parts using injection or infusion tecniques and is also available in high volume, industrial quantities.

‘We are proud of our decision to move towards bio based products,’ said Danu Chotikapanich, Co­bra's CEO. ‘The composites industry must promote sustainability to support a greener future for everyone.’

This story uses material from Sicominwith editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.