An elusive state of matter called superconductivity could be realized in stacks of sheetlike crystals just a few atoms thick, a trio of physicists has determined.
Superconductivity, the flow of electrical current without resistance, is usually found in materials chilled to the most frigid temperatures, which is impractical for most applications. It's been observed at higher temperatures–higher being about 100 kelvin or minus 280 degrees below zero Fahrenheit–in copper oxide materials called cuprate superconductors. But those materials are brittle and unsuitable for fabricating devices like circuits.
Researchers proposed a design for an artificially structured material that should support superconductivity at temperatures rivaling those seen for cuprates.
They considered a material made by interleaving two different types of crystal, one a semiconductor compound and the other a type of insulator. Two one-atom thick layers of the semiconductor compound molybdenum disulfide would be separated by a few-atom thick spacer made of boron nitride, and surrounded by additional boron nitride cladding.
This sets up a situation in which electrons and "holes" left by a missing electrons would accumulate in separate layers of the semiconductor compound in response to an electrical field. And yet these separated electrons and holes would be bound, at a distance, in states called indirect excitons.
These indirect excitons would form a gas with vanishing viscosity. That is, below a certain temperature, the gas would become superfluid. The physicists determined that superfluidity of indirect excitons would set up countercurrents that would not dissipate, a phenomenon called counterflow superconductivity.
Superfluidity and superconductivity are macroscopic manifestations of quantum phenomena, which are usually seen at the smallest physical scales.
The team's analysis reveals a general principle for creating "coherent states" like superfluidity and superconductivity that would emerge in similar materials created with layers of other semiconductor compounds such as tungsten disulfide or tungsten diselenide as well.
Such van der Waals structures are the subject of many investigations; this new analysis demonstrates that they also provide a new platform for exploring fundamental quantum phenomena.
Practical uses are possible as well; these materials could be used to develop electronic and optoelectronic circuits.
This story is reprinted from material from UC San Diego, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.