The toxicological impact of nanoparticles

28 February 2008
Download Type: Adobe PDF

Nanotechnology is a relatively new and vast field.

Even though nanotechnology is a fairly new field, nanomaterials are not. Au and Ag nanoparticles (NPs) were used in Persia in the 10th century BC to fabricate ceramic glazes to provide a lustrous or iridescent effect. This technique was then brought to Spain, where it was improved by the Moors during the 14th century, before finally spreading throughout much of Europe. In addition, over 5000 years ago, the Egyptians ingested Au NPs for mental and bodily purification. In all cases, the users did not know that they were NPs.