Researchers at Los Alamos National Laboratory's biggest magnet facility today met the grand challenge of producing magnetic fields in excess of 100 tesla while conducting six different experiments. The hundred-tesla level is roughly equivalent to 2 million times Earth's magnetic field.
"This is our moon shot, we've worked toward this for a decade and a half," said Chuck Mielke, director of the Pulsed Field Facility at Los Alamos.
The team used the 100-tesla pulsed, multi-shot magnet, a combination of seven coils sets weighing nearly 18,000 pounds and powered by a massive 1,200-megajoule motor generator. There are higher magnetic fields produced elsewhere, but the magnets that create such fields blow themselves to bits in the process. The system at Los Alamos is instead designed to work nondestructively, in the intense 100-tesla realm, on a regular basis. The Los Alamos facility is one of three campuses forming the National High Magnetic Field Laboratory (NHMFL).
Today's 100.75-tesla performance produced research results for scientific teams from Rutgers University, École Nationale Supérieure d'Ingénieurs de Caen (ENSICAEN), McMaster University, University of Puerto Rico, University of Minnesota, Cambridge University, University of British Columbia, and Oxford University. The science that we expect to come out varies with the experiment, but can be summarized as:
Quantum Phase transitions and new ultra high field magnetic states
Electronic Structure determination
Topologically protected states of matter
In recent experiments, said Mielke, "the new magnet has allowed our users and staff to pin down the upper critical field of a new form of superconductor, discover two new magnetically ordered states in a material that has eluded scientists for nearly 30 years, observe magneto-quantum oscillations in a high temperature superconductor to unprecedented resolution, determine a topological state of a new material, and discover a new form of magnetic ordering in an advanced magnetic material."
The LANL team set on August 18 last year a new world record for the strongest magnetic field ever delivered by a nondestructive magnet. The scientists achieved an enormous 97.4 tesla—a magnetic field nearly 100 times more powerful than the giant junkyard car-lifting magnets, and some 30 times stronger than the field delivered during a medical MRI scan. That record was broken this morning as the team ramped up the big magnet again, reaching 98.35 T, with an eye toward the afternoon's 3-digit event.
Mielke said that since the team's latest foray into magnetic fields above 90 tesla, they've demonstrated that they can measure:
Upper critical fields of superconductors—radio frequency contactless conductivity
Quantum magnetic transitions—magnetic susceptibility
Electrical resistivity—magnetotransport
Optical spectroscopy—visible light transmission
Crystallographic length change—fiber-optic dilatometry
"Now, at 100 tesla, we can focusing our efforts to get multiple user experiments completed in single magnet runs on the big magnets since they are so oversubscribed. More than a dozen people are working together to make this happen here at the Laboratory," said Mielke.
The ability to create pulses of extremely high magnetic fields nondestructively provides researchers with an unprecedented tool for studying a range of scientific questions: from how materials behave under the influence of very high magnetic fields, to research into the quantum behavior of phase transitions in solids.
Researchers can explore extremes of low temperature and high magnetic field, which will contribute to our understanding of superconductivity, magnetic-field-induced phase transitions, and so-called quantum critical points, in which small changes in materials properties at very low temperature have dramatic effects on physical behavior. The magnet could also be used as a nanoscale microscope.
This story is reprinted from material from Los Alamos National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.