It took marine sponges millions of years to perfect their spike-like structures, but research mimicking these formations may soon alter how industrial coatings and 3-D printed to additively manufactured objects are produced.
A molecular process developed by researchers at the Department of Energy’s Oak Ridge National Laboratory, paves the way for improved silica structure design by introducing microscopic, segmented screw-like spikes that can more effectively bond materials for commercial use.
The study authors said other applications of the screw-like spikes could include coatings for eyeglasses, television screens, commercial transportation and even self-cleaning windows and roofs in rural and urban environments.
Created by emulsion droplets applied to a silica particle’s surface, the new, segmented spikes offer an alternative tool for material scientists and engineers that can better maintain and fuse bonds within a variety of microstructures.
Combined with tetraethyl orthosilicate, an additive molecule, the emulsion droplets begin to produce rod-like spikes whose growth can be controlled for silica structures and configured into new materials.
The development of a segmented spike comes as an enhanced version of previous research conducted by the team. Sharma explained that the screw-like shape of these spikes was achieved when temperature control was incorporated with the spike growth on preformed particles.
In previous experiments, the spikes appeared in a rod-like, linear shape, preventing the silica from bending into the diverse shapes Sharma’s team sought to create from the particle seeds.
“If you try to use these linear ones, they will lie down like a pen does,” Sharma said. “They won’t stand. But if you have the segmented, spiky screws or smooth spiky screws, they will stand. They are the better shape.”
According to the authors, the segmented spike’s most direct application rests on interface engineering and the ongoing advancements in additive manufacturing, another significant ORNL research area.
With the spikes’ new shape, materials for bonding layers can maintain a stronger internal structure, lasting longer than previously used approaches.
Authors also experimented with a hybrid structure made from silica and titania, confirming that the silica-based spike growth can work for other oxide materials as well.
While they noted the hybrid’s use in future processes, the authors said the spectrum of possibilities remains wide open for future researchers to explore.
“We actually developed a process to create new structures, but we didn’t focus on one application when we did that,” Sharma said. “We looked at a range of applications where this could fit, and we are now trying to explore all those directions.”
This story is reprinted from material from Oak Ridge National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.