Researchers at UT Dallas have created new structures that exploit the electromechanical properties of specific nanofibers to stretch to up to seven times their length, while remaining tougher than Kevlar.
These structures absorb up to 98 joules per gram. Kevlar, often used to make bulletproof vests, can absorb up to 80 joules per gram. Researchers hope the structures will one day form material that can reinforce itself at points of high stress and could potentially be used in military airplanes or other defense applications.
“Our experiment is proof of the concept that our structures can absorb more energy before failure than the materials conventionally used in bulletproof armors.”Dr. Majid Minary, assistant professor of mechanical engineering, University’s Erik Jonsson School of Engineering and Computer Science.
The electricity generated by stretching the twisted nanofiber formed an attraction 10 times stronger than a hydrogen bond, which is considered one of the strongest forces formed between molecules.
“We reproduced this process in nanofibers by manipulating the creation of electric charges to result in a lightweight, flexible, yet strong material,” said Minary, who is also a member of the Alan G. MacDiarmid NanoTech Institute. “Our country needs such materials on a large scale for industrial and defense applications.”
For their experiment, researchers first spun nanofibers out of a material known as polyvinylidene fluoride (PVDF) and its co-polymer, polyvinvylidene fluoride trifluoroethylene (PVDF-TrFE).
Researchers then twisted the fibers into yarns, and then continued to twist the material into coils.
“It’s literally twisting, the same basic process used in making conventional cable,” Minary said.
Researchers then measured mechanical properties of the yarn and coils such as how far it can stretch and how much energy it can absorb before failure.
“Our experiment is proof of the concept that our structures can absorb more energy before failure than the materials conventionally used in bulletproof armors,” Minary said. “We believe, modeled after the human bone, that this flexibility and strength comes from the electricity that occurs when these nanofibers are twisted.”
The next step in the research is to make larger structures out of the yarns and coils, Minary said.
This story is reprinted from material from UT Dallas, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.