AESF's fall training schedule consists of the following: 

Course: Environmental Stewardship Parts 1 & 2 (Wastewater Treatment & Pollution Prevention)
Course Dates: September 20-23, 2010
Optional Exam: September 24, 2010
Course Hours: 8:00 a.m. - 5:30 p.m.
Location: Chicago, IL
Instructor: Frank Altmayer, MSF, AESF Fellow

Course: Hard Chrome
Course Dates: October 21-22, 2010
Optional Exam Date: October 23, 2010
Course Hours: 8:00 a.m. - 5:30 p.m.
Location: Philadelphia, PA
Instructor: TBD
 

Course: Electroplating and Surface Finishing (Certification Course)
Course Dates: November 1-4, 2010
Optional Exam Date: November 5, 2010
Course Hours: 8:00 a.m. - 5:30 p.m.
Location: Southern California
Instructor: Frank Altmayer, MSF, AESF Fellow