Columbia Chemical has been granted zinc nickel approval by General Motors for TRIVECTA NI-Z BLACK 70 with TRIVECTA BLACK SEALER 350 under the GMW 4700 Type B, BL specification. Columbia Chemical’s unique black all trivalent passivating conversion coating for electroplated zinc nickel alloy is now part of GM’s limited list of approved finishers for zinc nickel. NI-Z BLACK 70 with TRIVECTA BLACK SEALER 350 meets all of the GMW 4700 Type B, BL specification minimum requirements including 240 hours to white corrosion, 1,000 hours to red corrosion and 61 cycles of the cyclic test.

For more information, contact Mark Schario, Vice President of Technologies, Columbia Chemical Corporation, 1000 Western Drive, Brunswick, OH 44212, 330/225-3200, www.columbiachemical.com. Columbia Chemical is one of the world’s largest manufacturers of zinc and zinc-alloy plating additives.