COVENTYA, one of the world leaders in electroplating chemicals for surface treatment, is pleased to announce the obtainment of two new chemical approvals in the U.S.

Chrysler PS-12182 (decorative black Zn/Ni finish):
COVENTEC P7755B (PERFORMA 285+FINIDIP 728.2 or 728.3+FINIDIP 113)

GMW16730 (decorative black Zn/Ni finish):
COVENTEC P8755B (PERFORMA 560+FINIDIP 728.2 or 728.3+FINIDIP 113)
This is our second approval to this specification.

This latest GM approval will be added to the long list of COVENTYA approvals obtained with VW, Renault, PSA, Audi, Toyota, Fiat, Honda, Ford, Volvo, Nissan and GM.

For more information, please visit www.coventya.com.