"Our research found that all of these nanoscale mechanisms work together to give the alloy its toughness and strength."Robert Ritchie, Berkeley Lab
A team of researchers led by scientists from the US Department of Energy's Lawrence Berkeley National Laboratory (Berkeley Lab) has identified several mechanisms that make a new, cold-loving material one of the toughest metallic alloys ever.
The alloy is made of chromium, manganese, iron, cobalt and nickel, so scientists refer to it as CrMnFeCoNi. It's exceptionally tough and strong at room temperature, which translates into excellent ductility, tensile strength and resistance to fracture. And unlike most materials, the alloy becomes tougher and stronger the colder it gets, making it an intriguing possibility for use in cryogenic applications such as storage tanks for liquefied natural gas.
To learn its secrets, the Berkeley Lab-led team studied the alloy with transmission electron microscopy (TEM) as it was subjected to strain. The images revealed several nanoscale mechanisms that activate in the alloy, one after another, which together resist the spread of damage. Among the mechanisms are bridges that form across cracks to inhibit their propagation. Such crack bridging is a common toughening mechanism in composites and ceramics but is not often seen in unreinforced metals.
Their findings could guide future research aimed at designing metallic materials with unmatched damage tolerance. The research appears in a paper in Nature Communications.
"We analyzed the alloy in earlier work and found spectacular properties: high toughness and strength, which are usually mutually exclusive in a material," says Robert Ritchie, a scientist with Berkeley Lab's Materials Sciences Division who led the research with Qian Yu of China's Zhejiang University and several other scientists. "So in this research, we used TEM to study the alloy at the nanoscale to see what's going on."
In materials science, toughness describes a material's resistance to fracture, while strength describes a material's resistance to deformation. It's very rare for a material to be both highly tough and strong, but CrMnFeCoNi isn't a run-of-the-mill alloy. It's a star member of a new class of alloys developed about a decade ago that contains five or more elements in roughly equal amounts. In contrast, most conventional alloys have one dominant element. These new multi-component alloys are called high-entropy alloys because they consist primarily of a simple solid solution phase, and therefore have a high entropy of mixing.
High-entropy alloys are a hot topic in materials research, but have only recently been available in a suitable quality for study. In 2014, Ritchie and colleagues found that at very cold temperatures, when CrMnFeCoNi deforms, a phenomenon called ‘twinning’ occurs, in which adjacent crystalline regions form mirror arrangements of one another. Twinning likely plays a part in the alloy's incredible toughness and strength. But twinning isn't extensively found in the alloy at room temperature (except in the crack bridges), yet the alloy's toughness and strength is still almost off the charts.
"If we don't see twinning at room temperature, then what other mechanisms give the alloy these amazing properties?" asks Ritchie. To find out, the scientists subjected the alloy to several straining experiments at room temperature, and used TEM to observe what happens.
Their time-lapse images revealed two phenomena related to shear stress: slow-moving perfect dislocations that give the material strength, and fast-moving partial dislocations that enhance ductility. They also saw a phenomenon involving partial dislocations known as ‘three-dimensional stacking fault defects’, which involves changes to the three dimensional arrangement of atoms in the alloy. These faults are big barriers to dislocation, like placing a stack of bricks in front of a growing fissure, and serve to harden the alloy.
The images also captured the nanoscale version of chewing a mouthful of toffee and having your teeth stick together: in some cases, tiny bridges deformed by twinning are generated across a crack, which help prevent the crack from growing wider. "These bridges are common in reinforced ceramics and composites," says Ritchie. "Our research found that all of these nanoscale mechanisms work together to give the alloy its toughness and strength."
This story is adapted from material from the Lawrence Berkeley National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.