For the first time, low-cost titanium powders, developed by Metalysis, have been used to 3D print aerospace and automotive parts
Scientists have synthesized a novel form of titanium nitride, called titanic nitride, which has promising mechanical and optoelectronic properties.
Scientists have developed a fast, non-destructive optical method for analyzing defects in 2D materials
A lightweight sunshield has been developed to protect the mirrors and instruments aboard the James Webb Space Telescope from solar radiation.