Molybdenum oxide nanowires: synthesis & properties
Volume 14, Issues 7–8, Page 346–353
| Liqiang Mai, Fan Yang, Yunlong Zhao, Xu Xu, Lin Xu, Bin Hu, Yanzhu Luo, Hangyu Liu
Molybdenum oxide nanowires have been found to show promise in a diverse range of applications, ranging from electronics to energy storage and micromechanics. This review focuses on recent research on molybdenum oxide nanowires: from synthesis and device assembly to fundamental properties. The synthesis of molybdenum oxide nanowires will be reviewed, followed by a discussion of recent progress on molybdenum oxide nanowire based devices and an examination of their properties. Finally, we conclude by considering future developments.