Using various analytical techniques, researchers have established how hydrogen bonding plays a key role in the performance of perovskite solar cells.

Current research
 

News
 

A thin layer of fullerene molecules allows electrons to travel further than previously thought possible in organic solar cells and organic semiconductors.

News
 