Rapid advances in materials and manufacturing technology are making organic light-emitting diodes (OLEDs) the leading technology for a new generation of thinner, lighter, higher-resolution displays for computers, televisions, and small hand-held devices. In addition, OLEDs could enable the development of new display applications including flexible plastic display devices, displays embedded into clothes or wall hangings, and even head-mounted displays.