A waste-to-energy incineration plant in Norway is employing fibre reinforced plastic (FRP) composite chimney liners manufactured by Tunetanken AS of Denmar

Corrosion-resistant composite components are being used in a carbon capture and sequestration (CCS) unit recently installed by American Electric Power (AEP