In recent years we have seen significant progress from shape memory alloys (SMAs) to shape memory polymers (SMPs). In this paper, we summarize the most recent advances in SMMs. The focus is on the new features found in traditional SMMs, namely SMAs and SMPs, and a newly emerging type of SMM, namely shape memory hybrid (SMH), which enables enthusiasts to design SMMs with tailored properties/features for a particular application without the aid of experts (“do-it-yourself” manner).