Share

Related Links

News

Edible Nanostructures

19 September 2010

Sugar, salt, alcohol and a little serendipity led a Northwestern University research team to discover a new class of nanostructures that could be used for gas storage and food and medical technologies. And the compounds are edible.

The porous crystals are the first known all-natural metal-organic frameworks (MOFs) that are simple to make. Most other MOFs are made from petroleum-based ingredients, but the Northwestern MOFs you can pop into your mouth and eat, and the researchers have.

“They taste kind of bitter, like a Saltine cracker, starchy and bland,” said Ronald A. Smaldone, a postdoctoral fellow at Northwestern. “But the beauty is that all the starting materials are nontoxic, biorenewable and widely available, offering a green approach to storing hydrogen to power vehicles.”

“With our accidental discovery, chemistry in the kitchen has taken on a whole new meaning,” said Sir Fraser Stoddart at Northwestern. The implications of what Sir Fraser refers to as “Bob’s your uncle chemistry” go all the way from cleaner air to healthier living, and it all comes from a product that can be washed down the sink.

 Metal-organic frameworks are well-ordered, lattice-like crystals. The nodes of the lattices are metals (such as copper, zinc, nickel or cobalt), and organic molecules connect the nodes. Within their very roomy pores, MOFs can effectively store gases such as hydrogen or carbon dioxide, making the nanostructures of special interest to engineers as well as scientists.

 “The metal-organic framework technology has been around since 1999 and relies on chemicals that come from crude oil,” explained Ross S. Forgan, also a postdoctoral fellow in Stoddart’s lab and co-first author of the paper. “Our main constituent is a starch molecule that is a leftover from corn production.”

For their edible MOFs, the researchers use not ordinary table sugar but gamma-cyclodextrin, an eight-membered sugar ring produced from biorenewable cornstarch. The salts can be potassium chloride, a common salt substitute, or potassium benzoate, a commercial food preservative, and the alcohol is the grain spirit Everclear.

With these ingredients in hand, the researchers actually had set out to make new molecular architectures based on gamma-cyclodextrin. Their work produced crystals. Upon examining the crystals’ structures using X-rays, the researchers were surprised to discover they had created metal-organic frameworks -- not an easy feat using natural products.

“Symmetry is very important in metal-organic frameworks,” Stoddart said. “The problem is that natural building blocks are generally not symmetrical, which seems to prevent them from crystallizing as highly ordered, porous frameworks.”

It turns out gamma-cyclodextrin solves the problem: it comprises eight asymmetrical glucose residues arranged in a ring, which is itself symmetrical. The gamma-cyclodextrin and potassium salt are dissolved in water and then crystallized by vapor diffusion with alcohol.

The resulting arrangement -- crystals consisting of cubes made from six gamma-cyclodextrin molecules linked in three-dimensions by potassium ions -- was previously unknown. The research team believes this strategy of marrying symmetry with asymmetry will carry over to other materials.

The cubes form a porous framework with easily accessible pores, perfect for capturing gases and small molecules. The pore volume encompasses 54 percent of the solid body.

“We achieved this level of porosity quickly and using simple ingredients,” Smaldone said. “Creating metal-organic frameworks using petroleum-based materials, on the other hand, can be expensive and very time consuming.”

Stoddart added, “It is both uplifting and humbling to come to terms with the fact that a piece of serendipity could have far-reaching consequences for energy storage and environmental remediation on the one hand and food quality control and health care on the other.”

 

 

This article is featured in:
Characterization  •  Nanotechnology