Share

Related Links

Related Stories

  • A hard X-ray interferometer
    A novel type of hard X-ray interferometer employing a bilens system with two parallel arrays of compound refractive lenses has been developed by scientists from France and Russia. Under coherent illumination, the bilens generates two diffraction limited mutually coherent beams. When the beams overlap they produce an interference pattern with a fringe spacing ranging from tens of nanometres to tens of micrometres.
  • Integrated nanowire array sensor circuit is a first
    An integrated sensor circuit that is based on nanowire arrays and combining light sensors with electronics made from different crystalline materials, has been developed by scientists at the Lawrence Berkeley Laboratory of the U.S. Department of Energy and the University of California at Berkeley
  • Engineers build smart petri dish
    Device can be used to image cell growth continuously
  • Engineers solve longstanding problem in photonic chip technology
    Findings help pave way for next generation of computer chips
  • Atomic magnetometers for materials characterization
    Sensitive magnetometry has been established as a powerful technique for the characterization and testing of materials, with the most demanding applications relying on SQUID magnetometers operating at cryogenic temperatures. The recent development of compact, non-cryogenic atomic magnetometers with sub-femtotesla sensitivity and easy sample access has opened up a number of new possibilities.

News

Terrahertz moves to the near field

26 September 2008

Passing through materials that are opaque to visible light, terrahertz waves offer advantages in imaging applications

Passing through materials that are opaque to visible light, terrahertz waves offer advantages in imaging applications. However, near-field imaging, beneficial for achieving high spatial resolution and better sensitivity, can be problematic in the terrahertz region with the detector located remotely from the probe.

An integrated device combining aperture, probe and detector on a single semiconductor chip has been developed at the Advanced Device Laboratory, Saitama, Japan, removing the need for optical and mechanical alignments [Kawano et.al., Nature, doi: 10.1038/nphoton.2008.157].

Near-field imaging is well established in the visible and microwave regions but sensitivity is commonly degraded by the separation of detector and probe, allowing the influence of far-field waves. Near-field terrahertz systems use a small aperture, with a consequent weak field and small wave area, and a collecting tip that is prone to picking up the stronger far-field background signal.

The new device efficiently detects only the evanescent wave with a planar probe that is integrated with the detector, eliminating the need for separate waveguide and lens. The 8 μm aperture and planar probe, separated by a layer of silicon dioxide insulation, are deposited onto a GaAs/AlGaAs chip with a rectangular detector of 2D electron gas (2DEG) 60nm below the chip surface. The evanescent wave induces resistance heating of the 2DEG and, because it is a two-dimensional layer, it is unaffected by the far-field wave. The planar probe effectively changes the spatial distribution of the evanescent field so that it is better coupled to the detector in the same plane.

“A resolution of 9 μm has been obtained using the system and further improvements are expected with the use of a detector based on carbon nanotubes, expected to exhibit higher sensitivity and resolution as well as operating temperature improvements,” explains Yukio Kawano. The resulting sub-micron device could be used at room temperature and is likely to open up new applications in chemistry, physics and engineering.

 

This article is featured in:
Characterization