This review discusses the basics of MR imaging, the origin of SPION's unique magnetic properties, recent developments in MRI acquisition methods for detection of SPIONs, synthesis and post-synthesis processes that improve SPION's imaging characteristics, and the outlook of the translational potential of SPIONs.
Click here for the Full Text
Materials Today (2011) 14(7-8), 330-338