Shooting light a curve

16 August 2011

Berkeley lab researchers develop technique for dynamically controlling plasmonic Airy beams

One of the earliest lessons in science that students learn is that a ray or beam of light travels in a straight line. Students also learn that light rays fan out or diffract as they travel. Recently it was discovered that light rays can travel without diffraction in a curved arc in free space. These rays of light were dubbed “Airy beams,” after the English astronomer Sir George Biddell Airy, who studied what appears to be the parabolic trajectory of light in a rainbow.
 
Now, scientists with the Lawrence Berkeley National Laboratory (Berkeley Lab) have demonstrated the first technique that provides dynamic control in real-time of the curved trajectories of Airy beams over metallic surfaces. This development paves the way for fast-as-light, ultra-compact communication systems and optoelectronic devices, and could also stimulate revolutions in chemistry, biology and medicine.
 
The key to the success of this work was their ability to directly couple free-space Airy beams – using a standard tool of optics called a “grating coupler” – to quasi-particles called surface plasmon polaritons (SPPs). Directing a laser beam of light across the surface of a metal nanostructure generates electronic surface waves – called plasmons – that roll through the metal’s conduction electrons (those loosely attached to molecules and atoms). The resulting interaction between plasmons and photons creates SPPs. By directly coupling Airy beams to SPPs, the researchers are able to manipulate light at an extremely small scale beyond the diffraction limit.
 
“Dynamic controllability of SPPs is extremely desirable for reconfigurable optical interconnections,” says Xiang Zhang, the leader of this research. “We have provided a novel approach of plasmonic Airy beam to manipulate SPPs without the need of any waveguide structures over metallic surfaces, providing dynamic control of their ballistic trajectories despite any surface roughness and defects, or even getting around obstacles. This is promising not only for applications in reconfigurable optical interconnections but also for precisely manipulating particles on extremely small scales.”
 
 “Up to now, different plasmonic elements for manipulating surface plasmons were realized either through structuring metal surfaces or by placing dielectric structures on metals,” says Peng Zhang, lead author of the Optics Letters paper and member of Xiang Zhang’s research group. “Both approaches are based on the fabrication of permanent nanostructures on the metal surface, which are very difficult if not impossible to reconfigure in real time. Reconfigurability is crucial to optical interconnections, which in turn are crucial for high performance optical computing and communication systems. The reconfigurability of our technique is a huge advantage over previous approaches.”
 
Adds co-author Zhigang Chen, a principal investigator with the Department of Physics and Astronomy at San Francisco State University, “With the reconfigurability of our plasmonic Airy beams, a small number of optical devices can be employed to perform a large number of functions within a compact system. In addition, the unique properties of the plasmonic Airy beams open new opportunities for on-chip energy routing along arbitrary trajectories in plasmonic circuitry, and allows for dynamic manipulations of nano-particles on metal surfaces and in magneto-electronic devices.”
 
Dynamic control of the plasmonic Airy beams is provided by a computer-controlled spatial light modulator, a device similar to a liquid crystal display that can be used to offset the incoming light waves from a laser beam with respect to a cubic phase system mask and a Fourier lens. This generates a plasmonic Airy beam on the surface of a metal whose ballistic motion can be modified.
 
“The direction and speed of the displacement between the incoming light and the cubic phase mask can be controlled with ease simply by displaying an animation of the shifting mask pattern as well as a shifting slit aperture in the spatial light modulator,” Peng Zhang says. “Depending on the refresh rate of the spatial light modulator this can be done in real time. Furthermore, our spatial light modulator not only sets the plasmonic Airy beam into a general ballistic motion, it also enables us to control the Airy beam’s peak intensity at different positions along its curved path.”
 
The ability of the spatial light modulator to dynamically control the ballistic motions of plasmonic Airy beams without the need of any permanent guiding structures should open doors to a number of new technologies, according to Xiang and Peng Zhang and their collaborators. For example, in nano-photonics, it enables researchers to design practical reconfigurable plasmonic sensors or perform nano-particle tweezing on microchips. In biology and chemistry, it allows researchers to dynamically manipulate molecules.
 
This story is reprinted from material from Berkeley Lab, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.

 