In this article, we review the work performed and the trends in the development of environmental sensors on plastic and flexible foils. Our main focus is on the integration of temperature, humidity, and gas sensors on plastic substrates targeting low-power operation for wireless applications.
Click here for the Full Text
Materials Today (2011) 14(9), 416-423
doi: 10.1016/S1369-7021(11)70186-9