Seaweed polymer electrodes

09 September 2011

Improved lithium-ion batteries

 

By looking to Mother Nature for solutions, researchers have identified a promising new binder material for lithium-ion battery electrodes that could not only boost energy storage, but also eliminate the use of toxic compounds now used in manufacturing the components.
 
Known as alginate, the material is extracted from common, fast-growing brown algae. In tests so far, it has helped boost energy storage and output for both graphite-based electrodes used in existing batteries and silicon-based electrodes being developed for future generations of batteries.
 
The research, the result of collaboration between scientists and engineers at the Georgia Institute of Technology and Clemson University, was reported in Science Express.
 
"Making less expensive batteries that can store more energy and last longer with the help of alginate could provide a large and long-lasting impact on the community," said Gleb Yushin, an assistant professor in Georgia Tech's School of Materials Science and Engineering. "These batteries could contribute to building a more energy efficient economy with extended-range electric cars, as well as cell phones and notebook computers that run longer on battery power -- all with environmentally-friendly manufacturing technologies."
 
Working with Igor Luzinov at Clemson University, the scientists looked at ways to improve binder materials in batteries. The binder is a critical component that suspends the silicon or graphite particles that actively interact with the electrolyte that provides battery power.
 
"We specifically looked at materials that had evolved in natural systems, such as aquatic plants which grow in salt water with a high concentration of ions," said Luzinov, a professor in Clemson's School of Materials Science and Engineering. "Since electrodes in batteries are immersed in a liquid electrolyte, we felt that aquatic plants -- in particular, plants growing in such an aggressive environment as salt water -- would be excellent candidates for natural binders."
 
Finding just the right material is an important step toward improving the performance of lithium-ion batteries, which are essential to a broad range of applications, from cars to cell phones. The popular and lightweight batteries work by transferring lithium ions between two electrodes -- a cathode and an anode -- through a liquid electrolyte. The more efficiently the lithium ions can enter the two electrodes during charge and discharge cycles, the larger the battery's capacity will be.
 
Existing lithium-ion batteries rely on anodes made from graphite, a form of carbon. Silicon-based anodes theoretically offer as much as a ten-fold capacity improvement over graphite anodes, but silicon-based anodes have so far not been stable enough for practical use.
 
Among the challenges for binder materials are that anodes to be used in future batteries must allow for the expansion and contraction of the silicon nanoparticles, and that existing electrodes use a polyvinylidene fluoride binder manufactured using a toxic solvent.
 
The alginate is extracted from the seaweed through a simple soda (Na2CO3)-based process that generates a uniform material. The anodes can then be produced through an environmentally friendly process that uses a water-based slurry to suspend the silicon or graphite nanoparticles. The new alginate electrodes are compatible with existing production techniques and can be integrated into existing battery designs, Yushin said.
 
Use of the alginate may help address one of the most difficult problems limiting the use of high-energy silicon anodes. When batteries begin operating, decomposition of the lithium-ion electrolyte forms a solid electrolyte interface (SEI) on the surface of the anode. The SEI must be stable, allow lithium ions to pass through it, yet restrict the flow of fresh electrolyte.
 
With graphite particles, whose volume does not change, the SEI remains stable. However, because the volume of silicon nanoparticles changes during operation of the battery, cracks can form and allow additional electrolyte decomposition until the pores that allow ion flow become clogged, causing battery failure. Alginate not only binds silicon nanoparticles to each other and to the metal foil of the anode, but they also coat the silicon nanoparticles themselves and provide a strong support for the SEI, preventing degradation.
 
Thus far, the researchers have demonstrated that the alginate can produce battery anodes with reversible capacity eight times greater than that of today's best graphite electrodes. The anode also demonstrates a coulombic efficiency approaching 100 % and has been operated through more than 1000 charge-discharge cycles without failure.
 
This story is reprinted from material from Georgia Tech, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.

 

 