New approach to overcome next-generation superconductor hurdle

02 November 2011

Optimizing performance and minimizing risk

 

Researchers from North Carolina State University have developed a new computational approach to improve the utility of superconductive materials for specific design applications – and have used the approach to solve a key research obstacle for the next-generation superconductor material yttrium barium copper oxide (YBCO).
 
A superconductor is a material that can carry electricity without any loss – none of the energy is dissipated as heat, for example. Superconductive materials are currently used in medical MRI technology, and are expected to play a prominent role in emerging power technologies, such as energy storage or high-efficiency wind turbines.
 
One problem facing systems engineers who want to design technologies that use superconductive materials is that they are required to design products based on the properties of existing materials. But NC State researchers are proposing an approach that would allow product designers to interact directly with the industry that creates superconductive materials – such as wires – to create superconductors that more precisely match the needs of the finished product.
 
“We are introducing the idea that wire manufacturers work with systems engineers earlier in the process, utilizing computer models to create better materials more quickly,” says Dr. Justin Schwartz, lead author of a paper on the process and Kobe Steel Distinguished Professor and head of NC State’s Department of Materials Science and Engineering. “This approach moves us closer to the ideal of having materials engineering become part of the product design process.”
 
To demonstrate the utility of the process, researchers tackled a problem facing next-generation YBCO superconductors. YBCO conductors are promising because they are very strong and have a high superconducting current density – meaning they can handle a large amount of electricity. But there are obstacles to their widespread use.
 
One of these key obstacles is how to handle “quench.” Quench is when a superconductor suddenly loses its superconductivity. Superconductors are used to store large amounts of electricity in a magnetic field – but a quench unleashes all of that stored energy. If the energy isn’t managed properly, it will destroy the system – which can be extremely expensive. “Basically, the better a material is as a superconductor, the more electricity it can handle, so it has a higher energy density, and that makes quench protection more important, because the material may release more energy when quenched,” Schwartz says.
 
To address the problem, researchers explored seven different variables to determine how best to design YBCO conductors in order to optimize performance and minimize quench risk. For example, does increasing the thickness of the YBCO increase or decrease quench risk? As it turns out, it actually decreases quench risk. A number of other variables come into play as well, but the new approach was effective in helping researchers identify meaningful ways of addressing quench risk.
 
“The insight we’ve gained into YBCO quench behavior, and our new process for designing better materials, will likely accelerate the use of YBCO in areas ranging from new power applications to medical technologies – or even the next iteration of particle accelerators,” Schwartz says.
 
“This process is of particular interest given the White House’s Materials Genome Initiative,” Schwartz says. “The focus of that initiative is to expedite the process that translates new discoveries in materials science into commercial products – and I think our process is an important step in that direction.”
 
This story is reprinted from material from North Carolina State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

 

 

This article is featured in:
Electronic materials  •  Tools and Techniques