Study compares fundamental techniques for doping graphene sheets

08 November 2011

On the edge

 

Nanotechnology researchers at the Georgia Institute of Technology have conducted the first direct comparison of two fundamental techniques that could be used for chemically doping sheets of two-dimensional graphene for the fabrication of devices and interconnects.
 
Chemical doping is routinely used in conventional three-dimensional semiconductors to control the density of electron carriers that are essential to the operation of devices such as transistors.  But graphene, a semi-metal available in sheets just one atom thick, has properties very different from traditional materials such as silicon – though researchers say doping will still be needed for producing electronic devices.
 
The bad news is that electronic designers working with graphene won’t be able to simply apply what they’ve been doing with three-dimensional semiconductors – which would translate to vastly degraded material quality for graphene.  The good news, according to the study, is that graphene doping can be combined with other processes – and need be applied only to the edges of nanoscale structures being fabricated.
 
“We are learning how to manipulate these two-dimensional sheets of carbon atoms to get some very unusual results that aren’t available with any other material,” said James Meindl, director of Georgia Tech’s Nanotechnology Research Center, where the research was conducted.  “Doping graphene to try to influence its properties is important to being able to use it effectively.”
 
Details of the research were published online in the journal Carbon.
 
Because graphene sheets contain so few atoms by area, the substitution of elements such as oxygen or nitrogen for carbon atoms in the lattice – as in conventional doping – detracts from the high electron mobility and other properties that make the material interesting.  So the researchers are rethinking the doping process to take advantage of graphene’s unique properties.
 
“When we work with a three-dimensional semiconductor, we embed the dopant species in the bulk material and then fabricate it into a device,” said Kevin Brenner, a graduate research assistant in the Georgia Tech School of Electrical and Computer Engineering.  “With graphene, we will dope the material as we process it and fabricate it into devices or interconnects. Doping may be done as part of other fabrication steps such as plasma etching, and that will require us to reinvent the whole process.”
 
Using sheets of exfoliated graphene, Brenner and collaborators Raghu Murali and Yinxiao Yang evaluated the effectiveness of two different techniques: edge passivation by coupling electron-beam lithography with a common resist material, and adsorption from coating the surface of the material.  They found that the edge treatment, which chemically reacts with defects created when the material is cut, was a thousand times more efficient at producing carriers in the graphene sheets than the surface treatment.
 
Armed with basic information about graphene doping, the researchers hope to now begin producing devices to study how graphene actually performs.
 
“Now that we have made a start at understanding how to dope the material, the next step is to begin putting this into nanoscale devices,” Brenner said.  “We want to see what kind of performance we can get.  That may tell us where graphene’s niche could be as an electronic material.”
 
Meindl, who has worked with silicon since the dawn of integrated circuits, says it’s too early to predict where graphene will ultimately find commercial applications.  But he says the material’s properties are too interesting not to explore.
 
“The chances are that something very interesting and unique will develop from the use of graphene,” he said.  “But we don’t yet have the ability to predict what we will be able to do with this new material.
 
 
This story is reprinted from material from the GeorgiaTech, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

 

 