Researchers ink nanostructures with tiny ‘soldering iron’

10 November 2011

Thermal dip-pen nanolithography

Researchers with the U.S. Department of Energy (DOE)’s Lawrence Berkeley National Laboratory (Berkeley Lab) have shed light on the role of temperature in controlling a fabrication technique for drawing chemical patterns as small as 20 nanometers.  This technique could provide an inexpensive, fast route to growing and patterning a wide variety of materials on surfaces to build electrical circuits and chemical sensors, or study how pharmaceuticals bind to proteins and viruses.
 
One way of directly writing nanoscale structures onto a substrate is to use an atomic force microscope (AFM) tip as a pen to deposit ink molecules through molecular diffusion onto the surface.  Unlike conventional nanofabrication techniques that are expensive, require specialized environments and usually work with only a few materials, this technique, called dip-pen nanolithography, can be used in almost any environment to write many different chemical compounds.  A cousin of this technique — called thermal dip-pen nanolithography — extends this technique to solid materials by turning an AFM tip into a tiny soldering iron.
 
Dip-pen nanolithography can be used to pattern features as small as 20 nanometers, more than forty thousand times smaller than the width of a human hair.  What’s more, the writing tip also performs as a surface profiler, allowing a freshly-writ surface to be imaged with nanoscale precision immediately after patterning.
 
“Tip-based manufacturing holds real promise for precise fabrication of nanoscale devices,” says Jim DeYoreo, interim director of Berkeley Lab’s Molecular Foundry, a DOE nanoscience research center.  “However, a robust technology requires a scientific foundation built on an understanding of material transfer during this process.  Our study is the first to provide this fundamental understanding of thermal dip-pen nanolithography.”
 
In this study, DeYoreo and coworkers systematically investigated the effect of temperature on feature size. Using their results, the team developed a new model to deconstruct how ink molecules travel from the writing tip to the substrate, assemble into an ordered layer and grow into a nanoscale feature.
 
“By carefully considering the role of temperature in thermal dip-pen nanolithography, we may be able to design and fabricate nanoscale patterns of materials ranging from small molecules to polymers with better control over feature sizes and shapes on a variety of substrates,” says Sungwook Chung, a staff scientist in Berkeley Lab’s Physical Biosciences Division, and Foundry user working with DeYoreo.  “This technique helps overcome fundamental length scale limitations without the need for complex growth methods.”
 
This ‘nanoheater’ can then be used to heat up inks applied to the tip, causing them to flow to the surface for fabricating microscale and nanoscale features.  The group demonstrated this by drawing dots and lines of the organic molecule mercaptohexadecanoic acid on gold surfaces.  The hotter the tip, the larger the feature size the team could draw.
 
“We are excited about this collaboration with Berkeley Lab, which combines their remarkable nanoscience capabilities with our technology to control temperature and heat flow on the nanometer scale,” says co-author William P. King, a University of Illinois professor of mechanical sciences and engineering.  “Our ability to control the temperature within a nanometer-scale spot enabled this study of molecular-scale transport.  By tuning the hotspot temperature, we can probe how molecules flow to a surface.”
 
“This thermal control over tip-to-surface transfer developed by Professor King’s group adds versatility by enabling on-the-fly variations in feature size and patterning of both liquid and solid materials,” DeYoreo adds.
 
This story is reprinted from material from Berkeley Lab, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

 