News

New '3-D' transistors promising lighter laptops

New material could replace silicon

Researchers from Purdue and Harvard universities have created a new type of transistor made from a material that could replace silicon and have a 3-D structure instead of conventional flat computer chips.
 
The approach could enable engineers to build faster, more compact and efficient integrated circuits and lighter laptops that generate less heat than today's. The transistors contain tiny nanowires made not of silicon, like conventional transistors, but from a material called indium-gallium-arsenide.
 
The device was created using a so-called "top-down" method, which is akin to industrial processes to precisely etch and position components in transistors. Because the approach is compatible with conventional manufacturing processes, it is promising for adoption by industry, said Peide "Peter" Ye, a professor of electrical and computer engineering at Purdue.
 
A new generation of silicon computer chips, due to debut in 2012, will contain transistors having a vertical structure instead of a conventional flat design. However, because silicon has a limited "electron mobility" - how fast electrons flow - other materials will likely be needed soon to continue advancing transistors with this 3-D approach, Ye said.
 
Indium-gallium-arsenide is among several promising semiconductors being studied to replace silicon. Such semiconductors are called III-V materials because they combine elements from the third and fifth groups of the periodic table.
 
"Industry and academia are racing to develop transistors from the III-V materials," Ye said. "Here, we have made the world's first 3-D gate-all-around transistor on much higher-mobility material than silicon, the indium-gallium-arsenide."
 
Transistors contain critical components called gates, which enable the devices to switch on and off and to direct the flow of electrical current. In today's chips, the length of these gates is about 45 nanometers, or billionths of a meter. However, in 2012 industry will introduce silicon-based 3-D transistors having a gate length of 22 nanometers.
 
"Next year if you buy a computer it will have the 22-nanometer gate length and 3-D silicon transistors," Ye said. The 3-D design is critical because the 22-nanometer gate lengths will not work in a flat design.
 
"Once you shrink gate lengths down to 22 nanometers on silicon you have to do more complicated structure design," Ye said. "The ideal gate is a necklike, gate-all-around structure so that the gate surrounds the transistor on all sides."
 
However, further size reductions beyond 14 nanometers and additional performance improvements are likely not possible using silicon, meaning new designs and materials will be needed to continue progress, Ye said.
 
"Nanowires made of III-V alloys will get us to the 10 nanometer range," he said. The new findings confirmed that the device made using a III-V material has the potential to conduct electrons five times faster than silicon.
 
Creating smaller transistors also will require finding a new type of insulating layer essential for the devices to switch off. As gate lengths shrink smaller than 14 nanometers, the silicon dioxide insulator used in conventional transistors fails to perform properly and is said to "leak" electrical charge.
 
One potential solution to this leaking problem is to replace silicon dioxide with materials that have a higher insulating value, or "dielectric constant," such as hafnium dioxide or aluminum oxide.
 
In the new work, the researchers applied a dielectric coating made of aluminum oxide using a method called atomic layer deposition. Because atomic layer deposition is commonly used in industry, the new design may represent a practical solution to the coming limits of conventional silicon transistors.
 
Using atomic layer deposition might enable engineers to design transistors having thinner oxide and metal layers for the gates, possibly consuming far less electricity than silicon devices.
 
This story is reprinted from material from Purdue University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.