Visualizing electron pairing in iron superconductors

Findings support magnetic pairing theory

By measuring how strongly electrons are bound together to form Cooper pairs in an iron-based superconductor, scientists provide direct evidence supporting theories in which magnetism holds the key to this material’s ability to carry current with no resistance. Because the measurements take into account the electronic bands and directions in which the electrons are traveling, which was central to testing the theoretical predictions, this research strengthens confidence that this type of theory may one day be used to identify or design new materials with improved properties — namely, superconductors operating at temperatures far higher than today’s.

“In the best possible world you would be able to take this theory and plug in different chemical elements until you find a combination that should work as a superconductor at higher temperatures,” said Séamus Davis. Such materials could be used for real world, energy-saving technologies, such as zero-loss power transmission lines, without the need for expensive coolants

Scientists have been trying to understand the mechanism underlying so-called “high-temperature” superconductivity ever since discovering materials that could carry current with no resistance at temperatures somewhat above the operating realm of conventional superconductors, which must be chilled to near absolute zero (0 kelvin, or -273° Celsius). Though still mighty chilly, these high-Tc materials’ operating temperatures — some as high as 145K (-130° C) — offer hope that such materials could one day be designed to operate at room temperature.

One key to superconductivity is the formation of electron pairs. Scientists hypothesized that if these negatively charged particles have their magnetic moments pointing in opposite directions, they could overcome their mutual repulsion to join forces in so-called Cooper pairs — thus carrying current with no loss.

“Many people suspected you could take materials that naturally have alternating magnetic moments on adjacent electrons — antiferromagnetic materials — and convert them into superconductors,” Davis said. But to prove this conjecture hasn’t been possible with copper-based, or cuprate, superconductors — the first high-Tc superconductors discovered starting some 25 years ago. “You can make a robust antiferromagnetic cuprate insulator, but in that state it’s hard to get the magnetic electrons to pair and then move around and make a superconductor,” Davis said.

Then, in 2008, when iron-based superconductors were discovered, the idea that magnetism plays a role in high-Tc superconductivity was revived. But determining that role was a very complex problem. “In each iron atom there are five magnetic electrons, not just one,” Davis said. “And each, as it moves around the crystal, does so in a separate electronic band. In order to find out if the magnetic interactions between electrons are generating the superconductivity, you have to measure what’s called the anisotropic energy gap — how strongly bound together the electrons are in a pair — depending on the electrons’ directions on the different electronic bands.”

“It was our job to test those predictions,” Davis said. But at first, the techniques didn’t exist to make the measurements. “We had to invent them,” Davis said.

“This is the first experimental evidence direct from the electronic structure in support of the theories that the mechanism for superconductivity in iron-based superconductors is due primarily to magnetic interactions,” he said. The next step is to use the same technique to determine whether the theory holds true for other iron superconductors. “We and others are working on that now,” Davis said.

If those experiments show that the theory is indeed correct, the model could then be used to predict the properties of other elements and combinations — and ideally point the way toward engineering new materials and higher-temperature superconductors.

This story is reprinted from material from Brookhaven Lab, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.