Physicists at The University of Texas at Austin, in collaboration with colleagues in Taiwan and China, have developed the world’s smallest semiconductor laser, a breakthrough for emerging photonic technology with applications from computing to medicine.

Miniaturization of semiconductor lasers is key for the development of faster, smaller and lower energy photon-based technologies, such as ultrafast computer chips; highly sensitive biosensors for detecting, treating and studying disease; and next-generation communication technologies.

Such photonic devices could use nanolasers to generate optical signals and transmit information, and have the potential to replace electronic circuits. But the size and performance of photonic devices have been restricted by what’s known as the three-dimensional optical diffraction limit.

The device is constructed of a gallium nitride nanorod that is partially filled with indium gallium nitride. Both alloys are semiconductors used commonly in LEDs. The nanorod is placed on top of a thin insulating layer of silicon that in turn covers a layer of silver film that is smooth at the atomic level.

It’s a material that the Shih lab has been perfecting for more than 15 years. That “atomic smoothness” is key to building photonic devices that don’t scatter and lose plasmons, which are waves of electrons that can be used to move large amounts of data.

Nanolasers such as this could provide for the development of chips where all processes are contained on the chip, so-called “on-chip” communication systems. This would prevent heat gains and information loss typically associated with electronic devices that pass data between multiple chips.

This story is reprinted from material from
The University of Texas at Austin, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

Share this article

More services

 

This article is featured in:
Electronic materials  •  Optical materials  •  Tools and Techniques