Extracting uranium from seawater

New materials to help soak up metals

Fueling nuclear reactors with uranium harvested from the ocean could become more feasible because of a material developed by a team led by the Department of Energy's Oak Ridge National Laboratory.

The combination of ORNL's high-capacity reusable adsorbents and a Florida company's high-surface-area polyethylene fibers creates a material that can rapidly, selectively and economically extract valuable and precious dissolved metals from water. The material, HiCap, vastly outperforms today's best adsorbents, which perform surface retention of solid or gas molecules, atoms or ions. HiCap also effectively removes toxic metals from water, according to results verified by researchers at Pacific Northwest National Laboratory.

HiCap effectively narrows the fiscal gap between what exists today and what is needed to economically extract some of the ocean's estimated 4.5 billion tons of uranium. Although dissolved uranium exists in concentrations of just 3.2 parts per billion, the sheer volume means there would be enough to fuel the world's nuclear reactors for centuries.

The goal of extracting uranium from the oceans began with research and development projects in the 1960s, with Japan conducting the majority of the work. Other countries pursuing this dream include Russia, China, Germany, Great Britain, India, South Korea, Turkey and the United States. Many adsorbent materials have been developed and evaluated, but none has emerged as being economically viable.

What sets the ORNL material apart is that the adsorbents are made from small diameter, round or non-round fibers with high surface areas and excellent mechanical properties. By tailoring the diameter and shape of the fibers, researchers can significantly increase surface area and adsorption capacity. This and ORNL's patent pending technology to manufacture the adsorbent fibers results in a material able to selectively recover metals more quickly and with increased adsorption capacity, thereby dramatically increasing efficiency.

After the processing, scientists can place HiCap adsorbents in water containing the targeted material, which is quickly and preferentially trapped. Scientists then remove the adsorbents from the water and the metals are readily extracted using a simple acid elution method. The adsorbent can then be regenerated and reused after being conditioned with potassium hydroxide.

In a direct comparison to the current state-of-the-art adsorbent, HiCap provides significantly higher uranium adsorption capacity, faster uptake and higher selectivity, according to test results. Specifically, HiCap's adsorption capacity is seven times higher (146 vs. 22 grams of uranium per kilogram of adsorbent) in spiked solutions containing 6 parts per million of uranium at 20 degrees Celsius. In seawater, HiCap's adsorption capacity of 3.94 grams of uranium per kilogram of adsorbent was more than five times higher than the world's best at 0.74 grams of uranium per kilogram of adsorbent. The numbers for selectivity showed HiCap to be seven times higher.

This story is reprinted from material from Oak Ridge National Lab, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

Share this article