Related Links

News

Sliding metals show fluidlike behavior

New clues to wear

Researchers have discovered a swirling, fluidlike behavior in a solid piece of metal sliding over another, providing new insights into the mechanisms of wear and generation of machined surfaces that could help improve the durability of metal parts.

Studies using a microscope and high-speed camera revealed the formation of bumps, folds, vortexlike features and cracks on the metal surface. The findings were surprising because the experiment was conducted at room temperature and the sliding conditions did not generate enough heat to soften the metal. Numerous mechanical parts, from bearings to engine pistons, undergo such sliding.

The researchers are developing models to further study the phenomena and understand the wide-ranging consequences of such fluidlike flow in metals, Chandrasekar said. The findings might also lead to improved surface quality in materials processing.

The team observed what happens when a wedge-shaped piece of steel slides over a flat piece of copper. It was the first time researchers had directly imaged how sliding metals behave on the scale of 100 microns to 1 millimeter, known as the mesoscale.

The observations show how tiny bumps form in front of the steel piece, followed by the swirling vortexlike movement and then the creation of shallow cracks. The folding and cracking were most pronounced when the steel piece was held at a sharp angle to the copper surface.

The researchers hypothesize that the folding and cracking are due in part to a phenomenon similar to "necking," which happens as a piece of metal is stretched.

Researchers used a specialized laboratory setup that included a high-speed camera and equipment that applies force to the sliding metals. The behavior was captured in movies that show the flow in color-coded layers just below the surface of the copper specimen. Copper is commonly used to model the mechanical behavior of metals.

Metals are made of groups of crystals called grains. Metal surfaces that have smaller grains may be less susceptible to the folding and crack formation.

"We need to explore what role grain size plays," the researcher said. "We think there should be some grain size below which this folding mechanism might be less active. We need to explore why - under what conditions - solid metals behave like fluids."

This story is reprinted from material from Purdue University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

Share this article

More services

 

This article is featured in:
Characterization  •  Mechanical properties  •  Metals and alloys