X-ray laser reveals fast demagnetization

Surprising effects in ferromagnets

 

Scientists from TU Berlin, DESY and the University of Paris discovered a surprising effect in the demagnetisation of ferromagnetic materials at DESY’s free-electron laser FLASH. The team of researchers headed by Professor Stefan Eisebitt from Technische Universität Berlin is part of an international collaboration. The scientists found that electrons can move very quickly between areas with different magnetisation and thereby influence the demagnetisation of the material. The effect could play a decisive role in reducing the size of magnetic memories. “Optical demagnetisation is by far the quickest process to change magnetisation locally, and this in turn is the basis of magnetic storage,” Eisebitt explains. “Therefore, optical processes could help make magnetic memories faster in the future.” The scientists published the results of their study in the current issue of the journal “Nature Communications” (DOI 10.1038/ncomms2108).
 
The scientists discovered this effect while studying a phenomenon that has been a hot research topic for 20 years, ever since it was known that ferromagnets, for example magnetised iron, can be demagnetised extremely quickly when they are radiated with laser light pulses. In a few hundred femtoseconds (one femtosecond, 10-15 s, is a billionth of a millionth of a second) magnetisation breaks down and the ferromagnet loses its magnetic properties. After a while, magnetisation builds up again. When investigating this process at the X-ray laser FLASH, the scientists detected another mechanism that causes demagnetisation. It occurs when the material is divided into magnetic domains, which is often the case. “When bombarded with laser light, released electrons that speed through the material will break through the domain walls, thereby virtually changing sides. This way, they go from one domain into another domain with a different magnetic polarisation, causing the destruction of the local magnetisation,” explains junior scientist and lead author Bastian Pfau from TU Berlin. “Materials with nanometre-sized domains can this way develop another possibility of demagnetisation as soon as electrons become more mobile through the laser bombardment.” Such an interaction between two magnetic domains had already been assumed in theory, but has never before been observed.
 
The prerequisite of this kind of demagnetisation is that the basic material is divided into domains, which is usually the case with ferromagnets. Therefore, an unmagnetised iron bar consists of many microscopically small areas. Within these areas, the magnetisation has the same direction, but there is a random magnetisation of these miniature areas towards each other. When the iron bar is magnetised, for example when a magnetic field is applied from outside, the magnetic fields of the individual domains align in parallel and the whole iron bar becomes magnetic. “The magnetic moment is substantially supported through the spin, the angular momentum, of electrons,” explains Dr. Leonard Müller, one of the DESY scientists participating in this investigation. “Thus, the moving electrons will transport part of the magnetisation through the sample and cause modifications, especially at the domain walls.”
 
Scientists from TU Berlin, DESY, Helmholtz-Zentrum Berlin, the universities of Hamburg and Paris and from six additional research centres carried out these experiments at DESY’s free-electron laser FLASH in Hamburg. They investigated samples of a cobalt-platinum layer system containing tiny labyrinth-like magnetic domains. First, the working group induced the demagnetisation of the sample with an extremely short infrared laser pulse. After a “wait” of some hundred femtoseconds, the actual magnetisation of the sample was analysed with the help of FLASH X-ray laser light. “With the ultra-short X-ray flashes of less than 100 femtoseconds, FLASH is able to simultaneously determine the smallest modifications in size and properties of the magnetic domains,” said Dr. Christian Gutt from DESY.
 
These so-called pump-probe experiments, at which a system is first pumped and then probed after a certain period of time, are able to record extremely fast time lapses of chemical or physical modifications of a sample. However, it requires the exact synchronisation of two pulsed femtosecond lasers and the focusing of both at exactly the same spot of a tiny sample. “Ultra-short X-ray pulses as those of FLASH with their short waves are able to detect modifications in structures with the size of only a few nanometers,” said Professor Jan Lüning from the University of Pierre und Marie Curie in Paris.
 
The investigation of the scientists’ team showed that the initially sharp walls between the different domains became “blurred”, i.e. fuzzy, shortly after the infrared laser pulse – the limits became wider because the electrons broke through the domain walls. This became visible when, shortly after pumping, the probe X-ray pulses of the FLASH accelerator hitting the sample met a weaker deflection of their flight direction than before. Extensive simulations of the electron movement verified that this observation can be explained with a theoretically predicted demagnetisation mechanism through a change of domain by electrons.
 
“Our research shows that location and density of magnetic domain walls may influence the demagnetisation behavior,” explained Stefan Eisebitt. “This provides a new approach for the future to develop faster and smaller magnetic memories with a specific arrangement of magnetic nanostructures.”
 
This story is reprinted from material from DESY, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.
 

 