Stretching carbon nanotubes

For stronger materials

Researchers from North Carolina State University have developed new techniques for stretching carbon nanotubes (CNT) and using them to create carbon composites that can be used as stronger, lighter materials in everything from airplanes to bicycles.

By stretching the CNT material before incorporating it into a composite for use in finished products, the researchers straighten the CNTs in the material, which significantly improves its tensile strength – and enhances the stiffness of the composite material and its electrical and thermal conductivity.

State-of-the-art carbon fiber composites are currently used to build airplanes and other products where strong, lightweight materials are desirable. Lighter airplanes, for example, are more fuel efficient. However, researchers have long thought that if these composites could be made with CNTs they could be just as strong, but 10 times lighter. Or they could be the same weight, but 10 times stronger.

Creating a strong CNT composite requires four features. First, it needs long CNTs, which are more effective at carrying loads. Second, the CNTs need to be aligned in rows. Third, the CNTs in the material are held together by a polymer or resin, and you need to have a high ratio of CNTs to polymer in the finished composite material. Fourth, you need the CNTs to be as straight as possible, so that the material bears weight evenly.

“The new technique begins with a CNT array,” Zhu says, “which looks like a forest of CNTs growing up out of a flat substrate.” Because the aspect ratio of these CNTs is high, they are long and skinny – not rigid. That means the CNTs are leaning against each other in the array. “By grabbing the CNTs at one end of the array, we are able to pull them over onto their sides – and all of the other CNTs in the array topple in the same direction,” Zhu says. This results in CNTs with good alignment.

These aligned CNTs are then wound onto a rotating spool and sprayed with a polymer solution to bind the CNTs together. This creates a ribbon-like composite material that has a high percentage of CNTs by volume, which can in turn be used to make CNT composite structures for use in finished products like airplanes and bicycles. But that doesn’t address the need to straighten the CNTs.

To straighten the CNTs, Zhu and his team stretched the CNTs as the nanotubes are being pulled onto the rotating spool. This process improves the tensile strength of the CNT composite “ribbon” by approximately 90 percent (to an average of 3.5 gigapascals) and stiffness by more than 100 percent. By straightening the CNTs, the researchers were also able to almost triple the CNT composite’s thermal conductivity, to 40 watts per meter per kelvin. Electrical conductivity was increased by 50 percent to 1,230 siemens per meter.

This story is reprinted from material from NC State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

Share this article

More services

 

This article is featured in:
Carbon  •  Mechanical properties  •  Nanotechnology  •  Tools and Techniques