Nobody knows the remarkable properties of human skin like the researchers struggling to emulate it. Not only is our skin sensitive, sending the brain precise information about pressure and temperature, but it also heals efficiently to preserve a protective barrier against the world. Combining these two features in a single synthetic material presented an exciting challenge for Stanford Chemical Engineering Professor Zhenan Bao and her team.

Now, they have succeeded in making the first material that can both sense subtle pressure and heal itself when torn or cut.

In the last decade, there have been major advances in synthetic skin, said Bao, the study’s principal investigator, but even the most effective self-healing materials had major drawbacks. Some had to be exposed to high temperatures, making them impractical for day-to-day use. Others could heal at room temperature, but repairing a cut changed their mechanical or chemical structure, so they could only heal themselves once. Most importantly, no self-healing material was a good bulk conductor of electricity.

The researchers succeeded by combining two ingredients to get what Bao calls “the best of both worlds” – the self-healing ability of a plastic polymer and the conductivity of a metal.

They started with a plastic consisting of long chains of molecules joined by hydrogen bonds – the relatively weak attractions between the positively charged region of one atom and the negatively charged region of the next.

To this resilient polymer, the researchers added tiny particles of nickel, which increased its mechanical strength. The nanoscale surfaces of the nickel particles are rough, which proved important in making the material conductive. Tee compared these surface features to “mini-machetes,” with each jutting edge concentrating an electrical field and making it easier for current to flow from one particle to the next.

The result was a polymer with uncommon characteristics. “Most plastics are good insulators, but this is an excellent conductor,” Bao said.    

The next step was to see how well the material could restore both its mechanical strength and its electrical conductivity after damage.

The researchers took a thin strip of the material and cut it in half with a scalpel. After gently pressing the pieces together for a few seconds, they found the material gained back 75 percent of its original strength and electrical conductivity. The material was restored close to 100 percent in about 30 minutes. “Even human skin takes days to heal. So I think this is quite cool,” said Tee.

The team also explored how to use the material as a sensor. For the electrons that make up an electrical current, trying to pass through this material is like trying to cross a stream by hopping from stone to stone. The stones in this analogy are the nickel particles, and the distance separating them determines how much energy an electron will need to free itself from one stone and move to another.

Tee says that the material is sensitive enough to detect the pressure of a handshake. It might, therefore, be ideal for use in prosthetics, Bao said. The material is sensitive not only to downward pressure but also to flexion, so a prosthetic limb might someday be able to register the degree of bend in a joint.

Tee pointed out other commercial possibilities. Electrical devices and/or wires coated in this material could repair themselves and get electricity flowing again without costly and difficult maintenance, particularly in hard-to-reach places, such as inside building walls or vehicles.

Next up, Bao said the team’s goal is to make the material stretchy and transparent, so that it might be suitable for wrapping and overlaying on electronic devices or display screens.

This story is reprinted from material from Standford Engineering, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

Share this article

More services

 

This article is featured in:
Biomaterials  •  Electronic materials  •  Mechanical properties  •  Surface science