Cheap, strong lithium-ion batteries

New design includes porous silicon nanoparticles

Researchers at USC have developed a new lithium-ion battery design that uses porous silicon nanoparticles in place of the traditional graphite anodes to provide superior performance.

The new batteries — which could be used in anything from cellphones to hybrid cars — hold three times as much energy as comparable graphite-based designs and recharge within 10 minutes. The design, currently under a provisional patent, could be commercially available within two to three years.

Researchers have long attempted to use silicon, which is cheap and has a high potential capacity, in battery anodes. (Anodes are where current flows into a battery, while cathodes are where current flows out.)

The problem has been that previous silicon anode designs, which were basically tiny plates of the material, broke down from repeated swelling and shrinking during charging/discharging cycles and quickly became useless.

Last year, Zhou’s team experimented with porous silicon nanowires that are less than 100 nanometers in diameter and just a few microns long.

The tiny pores on the nanowires allowed the silicon to expand and contract without breaking while simultaneously increasing the surface area, which in turn allows lithium ions to diffuse in and out of the battery more quickly, improving performance.

Though the batteries functioned well, the nanowires are difficult to manufacture en masse. To solve the problem, Zhou’s team took commercially available nanoparticles — tiny silicon spheres — and etched them with the same pores as the nanowires. The particles function similarly and can be made in any quantity desired.

Though the silicon nanoparticle batteries currently last for just 200 recharge cycles (compared to an average of 500 for graphite-based designs), the team’s older silicon nanowire-based design lasted for up to 2,000 cycles, which was reported in Nano Lett last April.

Future research by the group will focus on finding a new cathode material with a high capacity that will pair well with the porous silicon nanowires and/or porous silicon nanoparticles to create a completely redesigned battery.

This story is reprinted from material from University of Southern California, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.

Share this article

More services

 

This article is featured in:
Electronic materials  •  Energy  •  Surface science