Related Links

  • Reichhold
  • Elsevier Ltd is not responsible for the content of external websites.

Related Stories

  • Study of FRP in infrastructure
    US and French researchers are teaming up to study the implementation of fibre reinforced plastic (FRP) composites in civil infrastructure such as bridges.
  • Construction composites worth US$3.1bn in 2013
    The European construction market for composite applications is estimated to reach US$3.1 billion in 2013, according to consultant Lucintel.
  • Understanding bio-materials
    A project led by UK organisations NetComposites and BRE will assess the environmental credentials of naturally-derived construction materials, including fibre reinforced plastics (FRP).
  • Nanoparticle films make for flexibility
    Nanoparticles typically exhibit low cohesion, making their use in thin films problematic. Scientists at Vanderbilt University have found a way of fabricating all-nanoparticle thin films that do not easily disintegrate, making them suitable for a wider range of applications than was previously the case [Hasan, et al., Chemical Communications 2009 25 3723].
  • Coatings go natural
    Ever since prehistoric days, humans have used natural paint systems to decorate caves, etc. However, after the introduction of cheaper base products such as mineral oils, the use of more expensive and environmentally friendly resources in paints and coatings declined.

News

Soy-based resin for SMC/BMC and pultrusion

16 February 2009

Reichhold has introduced a soy oil based resin, Polylite® 31325-00, suitable for sheet/ bulk moulding compound (SMC/BMC) and pultrusion.

The non-promoted, medium reactive, low viscosity unsaturated polyester moulding resin is derived in part from renewable resources (25%). It is intended as a general purpose moulding resin, and is said to yield laminates with mechanical properties and performance similar to general purpose SMC, BMC, and pultrusion resins.

Reichhold of Research Triangle Park, North Carolina, USA, says the Polylite31325-00 resin has been developed to enable composite manufacturers to incorporate raw materials based on renewable resources into their products.

Applications include window lineals, appliance components, agricultural Class A body panels and electrical boxes.

 