Share

Related Stories

  • Graphene replaces silicon
    Scientists have made a breakthrough toward creating nanocircuitry on graphene, widely regarded as the most promising candidate to replace silicon as the building block of transistors.
  • A manganite changes its stripes
    Colossal conductivity changes
  • GO nano
    Producing uniform graphene oxide
  • Patterning SWNTs
    Scientific and technological interest in one-dimensional nanomaterials, in particular carbon nanotubes, is a result of their fascinating properties and their ability to serve as templates for directed assembly.
  • Light scattering and nanoparticles
    Metal oxide nanoparticles are finding increasing application in the preparation of new nanocrystalline materials, with metal oxide composites being used to confer new electronic, magnetic and optical properties into material structures. Often these materials are formulated and processed as slurries or aqueous suspensions. One key parameter in controlling the properties of such colloidal nanoparticle systems is their particle size. Light scattering techniques are widely used for its determination.

News

Novel gels from polymer mixes

22 August 2009

The most widely studied and commercially important block copolymers are poly(ethylene oxide) and poly(propylene oxide) triblocks.

 

The most widely studied and commercially important block copolymers are poly(ethylene oxide) and poly(propylene oxide) triblocks. Known commercially as Pluronics, these copolymers are exploited for their gelling properties and are used widely in cosmetics, pharmaceuticals and industrial processes.

The ability to control the flow properties of these Pluronic block copolymers is important during processing and end-use. Using mixtures of Pluronic block copolymers is one method of manipulating structural and rheological properties such as gel stiffness and deformation under shear.

A new Anton-Paar Physica MCR501 rheometer at ISIS enabled scientists from the University of Reading to simultaneously measure both rheometry and small angle neutron scattering [Newby et al., J. Coll. Int. Sci. (2008) 329 54].

Pluronic block copolymers form micelles at the beginning of the gelling process. Once a sufficiently high micelle concentration is reached, lyotrophic liquid crystal phases are formed.

By using multiple techniques including small angle neutron scattering at ISIS and dynamic light scattering at the nearby Diamond Light Source the group determined how the formation of micelles and the packing density of the Pluronic block copolymer chains affects the gel phase diagram.

The results of the study give clear routes to modify the structure of Pluronic block copolymers and engineer their rheological properties for use in bio-medical product applications.

 

 