Related Links

Related Stories

  • Magnetricity: The new magnetic electricity
    A magnetic charge can behave and interact just like an electric charge in some materials, according to new research led by the London Centre for Nanotechnology which could lead to a reassessment of current magnetism theories, as well as significant technological advances.
  • Magnetricity is taken for a spin
    At long last there is experimental evidence that magnetic charges exist and that they have measurable currents or magnetricity, just like an electric charge [Bramwell et al., Nature (2009) 461, 956].
  • Quantum melting
    The quantum phase transition paradigm for a 1D Ising chain placed in a transverse applied magnetic field has been realised experimentally for the first time, at ISIS. [Coldea et al., Science (2010) 327, 177]
  • Quantum dots, and silicon herald new functionality
    Researchers from UCLA's Henry Samueli School of Engineering and Applied Science describe the creation of a new material incorporating spintronics that could help usher in the next generation of smaller, more affordable and more power-efficient devices. [Xiu et al., Nature Mat. (2010) 9, 337.]
  • Molecular puppets
    When it comes to charges, molecules of hydrogen are just too symmetrical.

News

Magnetricity: The new magnetic electricity

15 October 2009

A magnetic charge can behave and interact just like an electric charge in some materials, according to new research led by the London Centre for Nanotechnology

Research, published today in Nature [Bramwell et al., Nature (2009), 461] proves the existence of atom-sized magnetic charges called ‘magnetic monopoles’ that behave and interact just like more familiar electric charges. It also demonstrates a perfect symmetry between electricity and magnetism – a phenomenon dubbed ‘magnetricity' by the authors from the London Centre for Nanotechnology and STFC’s ISIS Neutron and Muon Source .

In order to prove experimentally the existence of magnetic current for the first time, the team mapped Onsager's 1934 theory of the movement of ions in water onto magnetic currents in a material called spin ice. They then tested the theory by applying a magnetic field to a spin ice sample at a very low temperature and observing the process using muon relaxation at ISIS, a technique which acts as a super microscope allowing researchers to understand the world around us at the atomic level.
The experiment allowed the team to detect magnetic charges in the spin ice (Dy2Ti2O7), to measure their currents, and to determine the elementary unit of the magnetic charge in the material. The monopoles they observed arise as disturbances of the magnetic state of the spin ice, and can exist only inside the material.
Professor Steve Bramwell, LCN co-author of the paper, said: “Magnetic monopoles were first predicted to exist in 1931, but despite many searches, they have never yet been observed as freely roaming elementary particles. These monopoles do at least exist within the spin ice sample, but not outside.
"It is not often in the field of physics you get the chance to ask 'How do you measure something?' and then go on to prove a theory unequivocally. This is a very important step to establish that magnetic charge can flow like electric charge. It is in the early stages, but who knows what the applications of magnetricity could be in 100 years time."
Dr Sean Giblin, instrument scientist at ISIS and co-author of the paper, added: “The results were astounding, using muons at ISIS we are finally able to confirm that magnetic charge really is conducted through certain materials at certain temperatures – just like the way ions conduct electricity in water.” 
 
 

 