Related Links

Related Stories

  • 2011 Acta Materialia Gold Medal
    The winner of the 2011 Acta Materialia Inc Gold Medal Award is Professor Jagdish (Jay) Narayan
  • The scientific symposium “Materials Challenges for Clean Energy in the New Millennium”
    The global energy problem is rapidly intensifying due to escalating competition for resources from emerging, populous countries such as China, India, and Brazil and compelling evidence pointing towards the imperative need for controlling greenhouse gas and carbon emissions.
  • A safe reaction
    Nuclear reactors might one day be constructed using materials that can self-heal following radiation damage, thanks to a materials study by scientists at Los Alamos National Laboratory.
  • A safe reaction
    Nuclear reactors might one day be constructed using materials that can self-heal following radiation damage, thanks to a materials study by scientists at Los Alamos National Laboratory.
  • The long and winding road to synthetic silk
    Unravelling the secret of silk's incredible strength

Feature

Discovery and design of nuclear fuels

22 December 2009
Marius Stan

To facilitate the discovery and design of innovative nuclear fuels, multi-scale models and simulations are used to predict irradiation effects on properties such as thermal conductivity, oxygen diffusivity, and thermal expansion. The multi-scale approach is illustrated using results on ceramic fuels, with a focus on predictions of point defect concentration, stoichiometry, and phase stability. The high performance computer simulations include coupled heat transport, diffusion, and thermal expansion, and gas bubble formation and evolution in a fuel element consisting of UO2 fuel and metallic cladding.

The second part of the paper is dedicated to a discussion of an international strategy for developing advanced, innovative nuclear fuels. Four initiatives are proposed to accelerate the discovery and design of new materials: (a) Create Institutes for Materials Discovery and Design, (b) Create an International Knowledgebase for experimental data, models (mathematical expressions), and simulations (codes), (c) Improve education and (d) Set up international collaborations.