Related Stories

  • Nano Snowman
    You're looking at the tiniest snowman ever built, 10 microns across.
  • Graphene replaces silicon
    Scientists have made a breakthrough toward creating nanocircuitry on graphene, widely regarded as the most promising candidate to replace silicon as the building block of transistors.
  • Moiré patterns in graphene
    Researchers have shown how atomic scale moiré patterns, which cause an interference pattern to appear when grids are overlaid askew, can measure how sheets of graphene are stacked and, crucially, reveal areas of strain.
  • The scientific symposium “Materials Challenges for Clean Energy in the New Millennium”
    The global energy problem is rapidly intensifying due to escalating competition for resources from emerging, populous countries such as China, India, and Brazil and compelling evidence pointing towards the imperative need for controlling greenhouse gas and carbon emissions.
  • AFM and combined optical techniques
    scanning probe microscopy has undergone rapid development to become an invaluable metric in the physical, biological, and materials sciences. One of the most exciting advances has been the integration of scanning probe techniques with optical microscopy. This paper will describe some of the basics of scanning probe and optical microscopy as well as some of the technical design challenges present when fusing these two imaging modalities. Examples of research problems solved with these combined techniques will be presented, with an emphasis on the advantages that each modality brings to the experiment.

News

Nano-snowman

09 February 2010

You're looking at the tiniest snowman ever built, 10 microns across.

It looks like a snowman, but this minuscule model — about a fifth the width of a human hair — is not made out of snow. It's constructed of two tiny tin beads that are usually used to calibrate an electron microscope, and welded together with platinum.

It's built by David Cox, a nanotech expert at the Quantum Detection Group of Britain's National Physical Laboratory. He's accustomed to working with small objects, and used his nano-particle manipulation tools to demonstrate the astonishing accuracy of his work.

A nanomanipulation system was used to assemble the parts 'by hand' and platinum deposition was used to weld all elements together. The snowman is mounted on a silicon cantilever from an atomic force microscope whose sharp tip 'feels' surfaces creating topographic surveys at almost atomic scales.

He bathed the snowman in blue light to give us this entertaining, snow-blown image. The remarkable flourish of his smiling snowman is its little happy face, carved into the top orb using a focused ion beam. That's no small feat.

 

 

This article is featured in:
Nanotechnology

 

Comment on this article