Thermopower has more energy

21 April 2010

A team of scientists at MIT have discovered a previously unknown phenomenon

This phenomenon can cause powerful waves of energy to shoot through minuscule wires known as carbon nanotubes. The discovery could lead to a new way of producing electricity, the researchers say.

The phenomenon, described as thermopower waves, “opens up a new area of energy research, which is rare,” says Strano, Associate Professor of Chemical Engineering [Choi et al., Nature Materials (2010), doi:10.1038/nmat2714]
Like a collection of flotsam propelled along the surface by waves traveling across the ocean, it turns out that a thermal wave — a moving pulse of heat — traveling along a microscopic wire can drive electrons along, creating an electrical current.
The key ingredient in the recipe is carbon nanotubes — submicroscopic hollow tubes made of a chicken-wire-like lattice of carbon atoms. These tubes, just a few billionths of a meter (nanometers) in diameter, are part of a family of novel carbon molecules, including buckyballs and graphene sheets, that have been the subject of intensive worldwide research over the last two decades.
In the new experiments, each of these electrically and thermally conductive nanotubes was coated with a layer of a reactive fuel that can produce heat by decomposing. This fuel was then ignited at one end of the nanotube using either a laser beam or a high-voltage spark, and the result was a fast-moving thermal wave traveling along the length of the carbon nanotube like a flame speeding along the length of a lit fuse. Heat from the fuel goes into the nanotube, where it travels thousands of times faster than in the fuel itself. As the heat feeds back to the fuel coating, a thermal wave is created that is guided along the nanotube. With a temperature of 3,000 kelvins, this ring of heat speeds along the tube 10,000 times faster than the normal spread of this chemical reaction. The heating produced by that combustion, it turns out, also pushes electrons along the tube, creating a substantial electrical current.
Combustion waves — like this pulse of heat hurtling along a wire — “have been studied mathematically for more than 100 years,” Strano says, but he was the first to predict that such waves could be guided by a nanotube or nanowire and that this wave of heat could push an electrical current along that wire.
When they wired up the carbon nanotubes with their fuel coating in order to study the reaction, a large resulting voltage peak that propagated along the wire was witnessed.

After further development, the system now puts out energy, in proportion to its weight, about 100 times greater than an equivalent weight of lithium-ion battery

 