LPW Technology researches powder for AM

LPW Technology, a supplier of PM for additive manufacturing (AM) applications, has acquired a Freeman Technology rheometer to research new powders and impr

Canadian Graphite producer Lomiko Metals and Graphene Laboratories Inc formed Graphene 3D Labs Inc to focus on the development of high-performance graphene

A team in the US is asking for investment in a small 3D printer that makes components from precious metal clay.

Sigma Labs Inc has extended its contract with Honeywell Aerospace to further demonstrate the capabilities of its PrintRite3D technology to make additive ma

Renishaw is collaborating with WEAF (West of England Aerospace Forum), to hold an Additive Manufacturing Focus Day at its headquarters in Gloucestershire,

rapid prototype + manufacturing (rp+m) says it can now 3D print metal prototypes and end parts, using an EOSINT M 280 direct metal laser sintering (DMLS) s

RaceWare Direct, a start-up company, has leveraged additive manufacturing technology to build their business.

The 2014 Additive Manufacturing Users Group (AMUG) conference, which takes place in Tucson, Ohio from 6-10 April, will include a full metals theme for the

Finnish coating technology specialist Picodeon Ltd has developed a short pulsed laser deposition technology (US PLD) for use in the application of gold and

Optomec has launched the Aerosol Jet 200 benchtop, suitable for research applications, such as prototyping small electronic devices, or developing and cert

Solid Concepts has made the world’s first 3D printed metal gun using a laser sintering process.

According to a new market research report, the additive manufacturing (AM) market is expected to grow at a CAGR of 13.5% from 2012 to 2017 to reach US$3,47

MetalForming magazine, the publication of the Precision Metalforming Association (PMA), will run a webinar on 12 December covering 3D printing with metals.

Connect with us
What’s coming up in additive manufacturing…
21
Jan ’21

 
11
Feb ’21

 
04
Mar ’21

 
25
Mar ’21