The NXG XII 600 printers incorporate 12 lasers with 1 kW power each and a build envelope of 600 x 600 x 600 mm.
The NXG XII 600 printers incorporate 12 lasers with 1 kW power each and a build envelope of 600 x 600 x 600 mm.

A European OEM has signed a Memorandum of Understanding (MoU) to purchase five new 3D printing machines, with the first machine delivery in 2022, according to manufacturer SLM Solutions.

The NXG XII 600 printers incorporate 12 lasers with 1 kW power each and a build envelope of 600 x 600 x 600 mm.

‘This MoU just two months after the launch is an exciting milestone for the company,’ said Sam O'Leary, CEO. ‘It validates our vision that the OEMs can implement innovative additive manufacturing technology for serial production into their business models.’