The aim of the two-year partnership is to improve the properties of materials used, and improve the processes for the design and cleaning of polymer, ceramic and metal parts while protecting the environment.

Prodways makes 3D printers and materials for a wide range of industrial and biomedical applications using photosensitive resins, technical ceramics and metals. 

CEA-Liten's goal is to improve the performance of materials and design new solutions that are economical, reliable and lightweight. The solutions use on multi-material systems and nanostructuring to improve material properties. The organisation has an R&D platform including a complete line of industrial and semi-industrial equipment so can carry out the entire process of producing these materials from metallic, ceramic and magnetic powders in a single building.