3D printing startup Carboni e Metalli, based in Italy, has developed a concept motorcycle featuring 3D printed carbon fiber and titanium parts.

The motorbike is based on the classic KTM 250GS design and features a carbon fiber sub-frame, a carbon fiber and 3D printed titanium rear swingarm, and a 3D printed alminum front fork mounts to name a few, the company said.