Abstract: Perovskite solar cells (PSCs) have emerged as a ‘rising star’ in recent years due to their high-power conversion efficiency (PCE), extremely low cost and facile fabrication techniques. To date, PSCs have achieved a certified PCE of 25.2% on rigid conductive substrates, and 19.5% on flexible substrates. The significant advancement of PSCs has been realized through various routes, including perovskite composition engineering, interface modification, surface passivation, fabrication process optimization, and exploitation of new charge transport materials. However, compared with rigid counterparts, the efficiency record of flexible perovskite solar cells (FPSCs) is advancing slowly, and therefore it is of great significance to scrutinize recent work and expedite the innovation in this field. In this article, we comprehensively review the recent progress of FPSCs. After a brief introduction, the major features of FPSCs are compared with other types of flexible solar cells in a broad context including silicon, CdTe, dye-sensitized, organic, quantum dot and hybrid solar cells. In particular, we highlight the major breakthroughs of FPSCs made in 2019/2020 for both laboratory and large-scale devices. The constituents of making a FPSC including flexible substrates, perovskite absorbers, charge transport materials, as well as device fabrication and encapsulation methods have been critically assessed. The existing challenges of making high performance and long-term stable FPSCs are discussed. Finally, we offer our perspectives on the future opportunities of FPSCs in the field of photovoltaics.

Critical review of recent progress of flexible perovskite solar cells
Read full text on ScienceDirect

DOI: 10.1016/j.mattod.2020.05.002