Bio-acceptable 0D and 1D ZnO nanostructures for cancer diagnostics and treatment
Volume 50, Issue , Page 533–569
| Andrés Galdámez-Martínez, Jorge Gutiérrez-Flores, Andrés Baca Ibañez, Pritam Kumar Panda, Guillermo Santana, Horacio Astudillo de la Vega, Mrutyunjay Suar, Citlaly Gutiérrez Rodelo, Ajeet Kaushik, Yogendra Kumar Mishra, Ateet Dutt
Abstract: As bioapplications of 0D and 1D zinc oxide (ZnO) seem a recent development, they have brought many exciting proposals showing exquisite signs as sensors and assay platforms offering biomolecular selectivity and sensitivity for cancer diagnosis and treatment. Cancer researchers are looking for diagnostic and molecular instruments to identify the cancer-causing agents and subtle molecular shifts. The inclusion of high-performance ZnO materials due to their intrinsic properties such as viability, bio-acceptability, high isoelectric point, tunable morphology, etc., is promising for targeted detection and treatment processes. More specifically, ZnO nanowires (NWs) have offered the opportunity to yield new types of approaches against targeted cancer in contrast to their 0D counterparts. The ability of ZnO NW sensors to identify the molecular features (i.e., biomarker) of cancer and their integration portability has the potential to revolutionize cancer diagnosis and patient health monitoring timely and efficiently. Despite being robust, tunable properties based on surface chemistry and eco-friendly, scalable opportunities are yet to be explored. This review considers captivating research advances to identify and understand fundamental properties and examine various biosensing approaches and nanomedicine (via performing targeted drug delivery or therapeutic) aspects utilizing them while paying attention to different size regimes of ZnO NWs. The high-performance role of 0D and 1D ZnO as biosensors, capture devices, cell imaging complexes, or treatment is addressed on the bases of the controlled functions such as enhanced adsorption, reactivity, surface chemistry, cytotoxicity, and biocompatibility in various biological systems and models. With a comparative viewpoint, 0D and 1D ZnO nanostructures are going to emerge as breakthrough candidates for diagnostics and treatment of cancer effectively and efficiently.
Read full text on ScienceDirect
DOI: 10.1016/j.mattod.2021.07.025
Share this journal article