Activating nano-bulk interplays for sustainable ammonia electrosynthesis
Volume 60, Issue , Page 31–40
| Bin Hua, Wei Wu, Lu-Cun Wang, Yong Ding, Märtha M. Welander, Robert A. Walker, Dong Ding
Abstract
Small changes in a catalyst’s composition, modification, and/or integration into a reactor can have significant yet often poorly understood effects on (electro)catalysis. Here we demonstrate the careful tailoring of Ru/La0.25Ce0.75O2−x catalysts through the post-synthesized hydrothermal treatment together with control over the Ru loadings to create hydroxyl groups and electronic restructuring for ammonia electrosynthesis. When integrated into a protonic ceramic electrolyzer, the in situ formed Ce3+−OH/Ru sites facilitate both the NN decoupling and NH formation at 400 °C and 1 bar of N2, boosting the ammonia production rate (2.92 mol h−1 m−2) up to 100-fold higher than the current state-of-the-art electrolyzers. Moreover, such catalysts and electrolyzer design concepts can be readily tuned to more complex applications such as coproducing ammonia and other chemicals with hydrocarbons as direct hydrogen sources. The creation of coordinated saturated support –OH/metal sites in the advanced electrolyzer offers an attractive approach for future clean-energy and green-chemical industries.

See full text for more information.
Read full text on ScienceDirect
DOI: 10.1016/j.mattod.2022.09.011
Share this journal article